{"id":"ningbo-08-rb5f5d51302d4","kind":"table-row","label":"Tensile Strain at Break | 150 527-2 | 50mm/min | % | 50","bbox":[0.06552,0.39795,0.9117,0.41279],"data":{"table":"ningbo-08-t2","row":2,"fields":[{"column":1,"header":[],"value":"Tensile Strain at Break","bbox":[0.06571,0.39826,0.26694,0.4157]},{"column":2,"header":[],"value":"150 527-2","bbox":[0.37778,0.39816,0.47232,0.41725]},{"column":3,"header":[],"value":"50mm/min","bbox":[0.54406,0.39795,0.65101,0.41455]},{"column":4,"header":[],"value":"%","bbox":[0.73511,0.39826,0.75975,0.41279]},{"column":5,"header":[],"value":"50","bbox":[0.86242,0.39971,0.89117,0.4157]}]},"method":"aligned-text","images":[],"pageId":"ningbo-08","sourceFile":"Green Petrochemistry-PP Material宁波PP手册_副本.pdf","page":8,"applicationExamples":[]}