{"id":"ningbo-19-r68b1eb17f61b","kind":"table-row","label":"Tensile Strain at Break | 150 527-2 | 50mm/min | % | ≥100","bbox":[0.06747,0.39805,0.90965,0.4157],"data":{"table":"ningbo-19-t2","row":2,"fields":[{"column":1,"header":[],"value":"Tensile Strain at Break","bbox":[0.06754,0.39805,0.26721,0.41744]},{"column":2,"header":[],"value":"150 527-2","bbox":[0.37969,0.40066,0.47247,0.41911]},{"column":3,"header":[],"value":"50mm/min","bbox":[0.54611,0.40083,0.64896,0.41603]},{"column":4,"header":[],"value":"%","bbox":[0.73511,0.39971,0.75975,0.4157]},{"column":5,"header":[],"value":"≥100","bbox":[0.86242,0.40262,0.90965,0.4157]}]},"method":"aligned-text","images":[],"pageId":"ningbo-19","sourceFile":"Green Petrochemistry-PP Material宁波PP手册_副本.pdf","page":19,"applicationExamples":[]}