Packaging

Two 100% PCR bottle grades, two property profiles

HDPE-GH6100 and HDPE-GH6200 have the same stated recycled content. Tensile and flow measurements give a buyer two more ways to compare them.

Packaging
Application illustration

Keep the test conditions beside the values

Under ISO 527-2 at 50 mm/min, the reported tensile strengths are 27.5 MPa and 26.2 MPa respectively. Retain the method and speed when comparing a second supplier’s data.

From the handbook
ObjectItemRecorded value
HDPE-GH6100Bottle body material PCR content100 %
HDPE-GH6200Bottle body material PCR content100 %
HDPE-GH6100Tensile strength27.5 MPa
HDPE-GH6100Melt mass-flow rate0.32 g/10 min
HDPE-GH6200Tensile strength26.2 MPa
HDPE-GH6200Melt mass-flow rate0.35 g/10 min

Return to the processing question

At 190 °C with a 2.16 kg load, the melt mass-flow rates are 0.32 and 0.35 g/10 min. Bring the bottle drawing and current process window into the sampling discussion.

Sources

← All articlesExplore with AI ↗